特性 |
|---|
| 成型收缩率 |
| 拉伸强度 |
| 断裂伸长率 |
| 弯曲强度 |
| 弯曲模量 |
| 悬臂梁缺口冲击 |
| 热变形温度 |
| 阻燃性能 |
| 表面电阻率 |
| 体积电阻率 |
| 密度 |
|
测试标准 |
|---|
| ASTM D955 |
| ASTM D638 |
| ASTM D638 |
| ASTM D790 |
| ASTM D790 |
| ASTM D256 |
| ASTM D648 |
| UL 94 |
| IEC 60093 |
| IEC 60093 |
| ASTM D792 |
|
测试条件 |
|---|
| 3.2mm |
| 50mm/min |
| 50mm/min |
| 2mm/min |
| 2mm/min |
| 3.2mm 23℃ |
| 1.82Mpa |
| 2mm |
| - |
| - |
| 23°C |
|
单位 |
|---|
| % |
| Mpa |
| % |
| Mpa |
| Mpa |
| J/m |
| °C |
| Class |
| Ω |
| Ω•m |
| kg/m3 |
|
PC5310 G2 |
|---|
| 0.3-0.5 |
| 75 |
| 5 |
| 110 |
| 3500 |
| 100 |
| 142 |
| HB |
| 1.00E+16 |
| 1.00E+14 |
| 1250 |
|
PC5310 G4 |
|---|
| 0.2-0.4 |
| 95 |
| 2 |
| 150 |
| 6000 |
| 136 |
| 145 |
| HB |
| 1.00E+16 |
| 1.00E+14 |
| 1320 |
|
PC5310 G6 |
|---|
| 0.2-0.4 |
| 125 |
| 2 |
| 165 |
| 8000 |
| 162 |
| 147 |
| HB |
| 1.00E+16 |
| 1.00E+14 |
| 1430 |
- ●上述数据是用注塑样品在23℃,湿度50%的条件下测得,数据为实验典型值,不作正式质保承诺。
- ●颜色产品的数据可能略有变化
| 加工工艺 |
|---|
| A6110 |
| PC5320G4 |
| PC5330G6 |
| 料筒温度 射嘴 |
|---|
| 260~290℃ |
| 280~300℃ |
| 290~300℃ |
| 料筒温度 前段 |
|---|
| 250~285℃ |
| 280~295℃ |
| 290~310℃ |
| 料筒温度 中段 |
|---|
| 250~280℃ |
| 280~290℃ |
| 290~300℃ |
| 料筒温度 后段 |
|---|
| 240~270℃ |
| 270~280℃ |
| 280~290℃ |
| 模具温度 |
|---|
| 60~90℃ |
| 60~90℃ |
| 60~100℃ |
| 背压压力 |
|---|
| 0.35~1.00Mpa |
| 0.35~1.00Mpa |
| 0.35~1.00Mpa |
| 螺杆速度 |
|---|
| 25-75Rpm |
| 25-75Rpm |
| 25-75Rpm |
| 干燥温度 |
|---|
| 100~110℃ |
| 100~110℃ |
| 100~120℃ |
| 干燥时间 |
|---|
| 4h |
| 4h |
| 4h |
- ●以上工艺参数仅供参考,具体要根据产品、注塑机和模具进行适当调整。